INDUSTRIAL PLASTICS
| PRODUCTS | GENERAL DESCRIPTIONS AND APPLICATIONS |
| NYLONS - Type 6 and Type 6.6 | Aramids family. It's made by a ring opening polymerisation from the monomer caprolactam . Uses : Fiber Thermoplastics. Type 6 - Melting temperature 215 º C Glass transition temperature : -40 º C Work temperature : 90 º C Type 6.6 - Melting temperature 280 º C Glass transition temperature: -50 º C Work temperature : 110 º C Sheets, tubes and rollers. |
| NYLON TYPE 6 |
Screws and Washers. |
| P.T.F.E. | Fluoropolymer resins. Have exceptional resistance to high temperature, chemical reaction, corrosion, stress cracking and low friction properties. Applications : Architecture fabrics. Chemical Industry. Electrical and Electronic Industry. Automobile Industry. Cabling materials Food Processing Semiconductor manufacturing Melting temperature : 320 º C. Glass transition temperature : -250 º C. Work temperature : 260 º C. Sheets, tubes and rollers. |
| P.V.C. POLY ( VINYL-CHLORIDE ) |
Uses : Thermoplastics. Monomer: Vinyl- chloride Polymerisation : Free radical chain polymerisation, Melting temperature : 110 º C. Glass transition temperature : -10 º C. Work temperature : 60 º C. Sheets, tubes an rollers |
| POLYETHILENE | Uses: Thermoplastics, fibers Monomer : Ethylene Unbreakable Melting temperature : 137 º C. Glass transition temperature : -130º C to -80º C Work temperature : 80 º C. Sheets and rollers. |
| POLYPROPYLENE | Uses: Thermoplastics, fibers, thermoplastics elastomers. Unbreakable Melting temperature : 174 º C Glass transition temperature : - 17 º C. Work temperature : 100 º C. Sheets and rollers. |
| SILICONE | Melting temperature : 260 º C Glass transition temperature : -260 º C. Work temperature : 220 º C. Sheets. |
| POLY ( METHYL METACRYLATE ) | Uses : Thermoplastics Polymerisation : Free radical vinyl polymerisation. Glass transition temperature : -120 º C PMMA transparent like glass an colours Sheets , tubes an rollers |
| POLICARBONATE | Polymerisation : Interfacial polymerisation Monomer : Bisphenol A Melting temperature : 150 Glass transition temperature : -100 º C Work temperature : 120 º C Unbreakable Sheets. |
| CELULAR POLYCARBONATE | Sheets. |
| POLYURETANES | Sheets, tubes an rollers. From 80º to 95º SHORE A |
| ALL KIND OF PARTS MACHINED ACCORDING TO DRAWINGS IN ANY ONE OF THE MATERIALS MENTIONED ABOVE |